ʻO Ceramicite DPF Honeycomb Ceramic 

Hōʻike Pōkole:

Kānana Kiko Uila Cordierite (DPF)
Hana ʻia ka kānana maʻamau o ka cordierite. Hāʻawi nā kānana Cordierite i ka maikaʻi o ke kānana maikaʻi, ʻano ʻē
pipiʻi (hoʻohālikelike me ka kānana kahe kahe o ka paia). ʻO ka drawback nui ka cordierite i kahi pae heheʻe haʻahaʻa.


ʻIke kikoʻī

Nā huahana huahana

Kumumanaʻo hana

Ma ka hoʻokau ʻana i nā kinoea hoʻoluhi ma o nā paia ma waena o nā kahawai o ka DPF, waiho ʻia ka mea nui i nā paia, no laila e hōʻemi ana i ka nui o ka ea o ka ea.

Hoakaka

Nui CPSI Volume (L)
φ118 * 152.4 100/200 1.67
φ118 * 254 100/200 2.78
φ127 * 152.4 100/200 1.93
φ127 * 180 100/200 2.3
φ127 * 254 100/200 3.22
φ144 * 152.4 100/200 2.49
φ144 * 203 100/200 3.31
φ144 * 254 100/200 4.44
φ144 * 305 100/200 4.97
φ190 * 152.4 100/200 4.32
φ190 * 203 100/200 5.76
φ190 * 305 100/200 8.65
φ240 * 240 100/200 10.9
φ240 * 305 100/200 13.8
φ250 * 305 100/200 14.97
φ267 * 267 100/200 14.22
φ267 * 305 100/200 14.95
φ286 * 305 100/200 17.07
φ286 * 355 100/200 19.6
φ305 * 305 100/200 22.8
φ330 * 381 100/200 32.59
Nā Palapala ʻĀpana ʻIkepili
Nā Pono: Cordierite wt% ≥90 94
Coefficient o Thermal Expansion (20-800 ℃) cm / cm / ℃ ≤1.8 * 10 ≤1.5 × 10-6
Thermal paʻa (20-650 ℃) manawa 1 3
Hōʻaleʻale i ka Mahana ≥1420 1440
Ka ikaika o ka compression Nā Lōʻihi MPa 16 16.9
Papamoe MPa 5 6.2
Kaumaha kikoʻī Kg / L 0.45-0.55 0.45-0.5
ʻO Porosity % 40-45 41
Lāki lawe omo wai % 23-25 23.8